Research Article

Metallurgical and Machinability Characteristics of Wrought and Selective Laser Melted Ti-6Al-4V

Table 3

Details of the machining test.

Cutting conditionsMachining time [24]
Wrought Ti-6Al-4VSLM Ti-6Al-4V

= 60 m/min378378
= 120 m/min9090
= 180 m/min14416

Test was stopped due to high tool wear that resulted in vibrations and drastic increase in cutting forces.