Physical Characteristics and Technology of Glass Foam from Waste Cathode Ray Tube Glass

Figure 8

Microscopy images of sintered pellets (5x) at (a) 650°C, (b) 750°C, 6–8 mm, (c) 800°C, 6–8 mm, 10 min, (d) 850°C, 6–8 mm, 5 min, (e) 900°C, 7.5 min 2–4 mm, and (f) 900°C, 7.5 min 6–8 mm.