Figure 9

SEM micrographs of sintered pellets. (a) VI 1 c –850°C, 5 min, 6–8 mm, (b) VII 1 c –900°C, 5 min, 6–8 mm, (c) VII 1 c –900°C, 5 min, 6–8 mm: wall of the pellet, and (d) V 3 c –800°C, 10 min, 6–8 mm.