Research Article

Fabrication of Thermoelectric Sensor and Cooling Devices Based on Elaborated Bismuth-Telluride Alloy Thin Films

Table 2

EDX analysis of Bi2Te3 thin films at different .

Temperature (°C)% Bi% Te

39.92360.077
39.54060.460
39.60260.398
39.75160.249