Splitting tensile strength of 0%, 10%, 15%, and 20% OPS replacement concrete.

Splitting tensile strength (N/mm2)
Mix proportions0% replacement 10% replacement15% replacement20% replacement

1 : 1.65 : 2.452.962.502.302.07
1 : 2.5 : 3.32.822.362.181.94
1 : 3.3 : 4.22.582.141.961.73