Research Article
Sodium Sulphate Effect on Cement Produced with Building Stone Waste
Figure 5
(a) SEM microstructures of waste MP blended cement MP1 mortar bars after exposure to very severe (13500 mg/L) Na2SO4 solution for 90 days. (b) SEM microstructures of waste MP blended cement MP2 mortar bars after exposure to very severe (13500 mg/L) Na2SO4 solution for 90 days. (c) SEM microstructures of waste MP blended cement MP3 mortar bars after exposure to very severe (13500 mg/L) Na2SO4 solution for 90 days.
(a) |
(b) |
(c) |