Research Article

Optimization of Cutting Parameters during Dry Turning of Austenitic Stainless Steel Using nc-AlTiN/Si3N4, TiAlN, and TiN Coated Inserts

Figure 2

Wear images of inserts at = 250 m/min. and = 0.3 mm/rev.
(a)
(b)