Influence of Grain Boundary Character and Annealing Time on Segregation in Commercially Pure Nickel

Figure 3

(a) 3D atom-by-atom LEAP reconstructions of specimen 1 SGB; point size = 1.5 and the percentage of ions shown is 100% except for Ni (0.1%) and Al (50%). (b) 3D reconstructions of specimen 1 RGB; point size = 1.5 and the percentage of ions shown is 100% except for Ni at 0.10%, Al at 50%, and Si at 50%.