Results from N2 sorption characterization.

SampleSurface area (m2g-1)Pore volume (cm3 g-1)Average meso-/macropore size (nm)c
SBET%%Vtotal%%

Nano-porous Fe2O33543111%30189%0.290.027%0.2793%7

BET surface area (), surface area of micropores () and surface area of meso-/macropores () determined with the t-plot method.
The percentage data denotes the percentage of surface area of micropores or meso- and macropores relative to the total surface area.
Total pores volume (), micro volume () determined with the t-plot method. The percentage data denote the percentage of pore volume of micropores relative to the total pore volume.
Average meso-/macropores size () determined from the N2 desorption data with NLDET model.