Research Article

Comparative Assessment of Antimicrobial Efficiency of Ionic Silver, Silver Monoxide, and Metallic Silver Incorporated onto an Aluminum Oxide Nanopowder Carrier

Table 3

Physical properties of the Al2O3-Ag+, Al2O3-Ag2O, and Al2O3-Ag nanopowders produced by the thermal decomposition (700°C, 24 h) followed by reduction (H2, 700°C, 2 h).

Sample numbers
(Ag concentration)
Al2O3-Ag+Al2O3-Ag2OAl2O3-Ag
S BET/m2g−1V BJH × 10−3/m3g−1D BJH/nmS BET/m2g−1V BJH × 10−3/m3g−1D BJH/nmS BET/m2g−1V BJH × 10−3/m3g−1D BJH/nm

0 (0.00 wt%)252,600,8354169,600,7588
1 (0.30 wt%)118,500,50625161,800,6326148,500,61611
2 (1.35 wt%)198,600,8082228,101,34622208,001,19911
3 (2.84 wt%)151,300,4905175,800,6198157,600,6427
4 (12.55 wt%)228,000,5184178,600,5396172,900,4566