DSC and WAXD results of PLLA and its nanocomposites.

g-SBA-15 content
(wt%)
(°C)Crystallinity of PLLAb(%)

0180.130.7
5a176.033.6
5176.829.2
10177.329.8
15177.827.9

Nongrafted.
bDetermined by WAXD.