Research Article
Studies on Ion-Exchange Properties of Polyaniline Zr(IV) Tungstoiodophosphate Nanocomposite Ion Exchanger
Table 2
Conductivity of polyaniline Zr(IV) tungstoiodophosphate ion exchanger at different temperatures.
| Temp. (°C) | | | (Scm−1) | 1000/T (K) | |
| 100 | 0.95 | 41.9 | 4.76 | 2.681 | −5.3475 | 95 | 0.68 | 35.2 | 2.86 | 2.717 | −5.8569 | 90 | 0.54 | 30.9 | 2.00 | 2.755 | −6.2146 | 85 | 0.49 | 28.0 | 1.64 | 2.793 | −6.4131 | 80 | 0.45 | 25.1 | 1.32 | 2.833 | −6.6301 | 75 | 0.44 | 18.9 | 1.02 | 2.874 | −6.8879 | 70 | 0.41 | 16.3 | 0.80 | 2.916 | −7.1309 | 65 | 0.37 | 14.5 | 0.64 | 2.959 | −7.354 | 60 | 0.33 | 12.1 | 0.49 | 3.003 | −7.6211 | 55 | 0.29 | 10.8 | 0.37 | 3.049 | −7.9020 | 50 | 0.26 | 9.2 | 0.29 | 3.096 | −8.1456 | 45 | 0.21 | 7.1 | 0.18 | 3.145 | −8.6226 | 40 | 0.18 | 5.3 | 0.11 | 3.195 | −9.1150 | 35 | 0.16 | 4.4 | 0.08 | 3.247 | −9.4335 |
|
|