Research Article

Effects of Thermal and Solvent Aging on Breakdown Voltage of TPE, PBT/PET Alloy, and PBT Insulated Low Voltage Electric Wire

Figure 7

Microphotographs (200x) of the surface of extruded insulation layer after solvent aging at 120°C for 6 h.
493731.fig.007a
(a) At 120°C for 6 h
493731.fig.007b
(b) At 120°C for 6 h in xylene
493731.fig.007c
(c) At 120°C for 6 h in NMP