Synthesis and Characterization of Polyesteramide Hot Melt Adhesive from Low Purity Dimer Acid, Ethylenediamine, and Ethanolamine

Table 5

Thermal properties obtained for the prepared PEA HMAs.

Sample name (°C) (°C) (J/g) (°C) (J/g)

PEA04.2697.616.7783.838.17
PEA10−1.9281.9915.1874.145.70
PEA20−6.2972.8715.0570.093.87
PEA30−6.5872.589.6864.522.40