Research Article

Weatherability of Polypropylene by Accelerated Weathering Tests and Outdoor Exposure Tests in Japan

Figure 12

Changes in PP flexural strength resulting from outdoor exposure test and accelerated weathering test machines on the basis of PE-RS CI. are sample codes as indicated in Table 1. ■: outdoor exposure; others; same as Figure 6.