Research Article

Reuse Feasibility of Electrocoagulated Metal Hydroxide Sludge of Textile Industry in the Manufacturing of Building Blocks

Figure 6

Relationship between weight loss and shrinkage on ignition of NBB at (a) 950°C, (c) 1000°C, and (e) 1050°C and PBB at (b) 1000°C and (d) 1050°C at different EMHS percentages.
686981.fig.006a
(a)
686981.fig.006b
(b)
686981.fig.006c
(c)
686981.fig.006d
(d)
686981.fig.006e
(e)