Research Article

Study of Structure and Electro-Optical Characteristics of Indium Tin Oxide Thin Films

Figure 2

SEM images of ITO thin film with a thickness of 199 nm: (a) as-deposited, (b) annealed at 600°C.
408182.fig.002a
(a)
408182.fig.002b
(b)