Research Article

Corrosion and Leaching Behaviours of Sn-0.7Cu-0.05Ni Lead-Free Solder in 3.5 wt.% NaCl Solution

Figure 11

SEM image of lead-free solder alloy after 7, 15, and 30 days leaching measurement in 3.5 wt.% NaCl solution.