Research Article

Corrosion and Leaching Behaviours of Sn-0.7Cu-0.05Ni Lead-Free Solder in 3.5 wt.% NaCl Solution

Figure 7

Atomic Absorption Spectroscopy (AAS) results on Tin (Sn) leaching from lead-free solder alloy and joint after 30 days.