Structural and Kinetic Hydrogen Sorption Properties of Zr0.8Ti0.2Co Alloy Prepared by Ball Milling

Figure 1

XRD patterns of the activated Zr0.8Ti0.2Co samples after ball milling for different time. (i) 0 h; (ii) 2 h; (iii) 4 h; (iv) 6 h; (v) 8 h.