Review Article
Biodegradable Magnesium Alloys Developed as Bone Repair Materials: A Review
Figure 4
SEM images of sample surface morphology before (a) WE42, (b) WE42-MAO, and (c) WE42-MAO/PLLA and after (d) WE42, (e) WE42-MAO, and (f) WE42-MAO/PLLA were submerged in Hank’s solution at 37°C (pH = 7.4) [57].
(a) |
(b) |
(c) |
(d) |
(e) |
(f) |