Research Article
The Effect of EBM Process Parameters on Porosity and Microstructure of Ti-5Al-5Mo-5V-1Cr-1Fe Alloy
Figure 12
Microstructure of the specimens fabricated with different energy inputs and with the same cathode current (4.5 mA): (a) 20 J/mm3, (b) 30 J/mm3, (c) 40 J/mm3, and (d) 50 J/mm3; arrow indicates build direction.
(a) |
(b) |
(c) |
(d) |