Research Article
Evaluation of the Dislodgement Resistance of a New Pozzolan-Based Cement (EndoSeal MTA) Compared to ProRoot MTA and Biodentine in the Presence and Absence of Blood
Figure 1
Patterns of bond failure: (a) mixed, (b) adhesive, and (c) cohesive.
(a) |
(b) |
(c) |