Microstructure and Mechanical Properties of Microwave Sintered ZrO2 Bioceramics with TiO2 Addition
Figure 7
Optical microscope of the ZrO2 ceramics with addition of 5 wt% TiO2 contents sintered at (a) 1150°C, (b) 1200°C, (c) 1250°C, and (d) 1300°C (the scale bar is 20 μm.).