Printing parameters.

ParametersValues/settings

MaterialPLA, ABS
Quality: layer height0.1–0.2 mm
Shell: wall thickness1 mm
Infill20%
Printing temperature215°C (PLA)–255°C (ABS)
Diameter1.75 mm
Flow100%
Print speed400 mm/s
Travel speed120 mm/s
Build plate adhesion typeRaft
Raft air gap 0.3 mm
Initial layer Z overlap 0.15 mm