Long Term Compression Strength of Mortars Produced Using Coarse Steel Slag as Aggregate

Table 2

Composition, LOI, and density of CEII/B-LL and SS. “Others” indicates the cumulative quantity of all oxides determined in quantity lower than 0.1 wt%.

ComponentCEMIIB-LL (wt%)SS (wt%)

CaO62.338.2
SiO219.814.8
Al2O34.27.4
MgO2.511.7
Na2O0.6
K2O1.1
Fe2O33.29.8
MnO0.610.4
Cr2O32.0
V2O50.8
P2O51.2
2.9
Others2.83.7
Free lime1.9
LOI (%)4.25
Density (g/cm3)2.463.29

The amount of free CaO was previously measured following the ethylene glycol method.