Atterberg limits of the tested specimen.
| Calcium carbide slag content (%) | Maximum (%) | Minimum (%) | Variation magnitude (%) | Liquid limit | Number of cycles | Plastic limit | Number of cycles | Liquid limit | Number of cycles | Plastic limit | Number of cycles | Liquid limit | Plastic limit |
| 6 | 34.23 | 7 | 22.06 | 10 | 31.88 | 10 | 21.08 | 7 | 7.37 | 4.65 | 8 | 33.92 | 24.36 | 32.15 | 22.82 | 5.50 | 6.75 | 10 | 33.51 | 24.75 | 32.02 | 23.66 | 4.59 | 4.60 | 12 | 34.06 | 25.11 | 32.28 | 23.44 | 5.55 | 7.12 | 14 | 34.39 | 25.65 | 32.49 | 24.26 | 5.58 | 5.73 |
|
|