Experimental and Theoretical Study of a New Technique for Mixing Self-Compacting Concrete with Marble Sludge Grout
Table 7
The different mixing methods.
| Concrete reference | Dry mixing | Wet mixing | End of mixing | 1 min | 1.5 min | 2.5 min | Total 5 min |
| SCC1 procedure 1 | Aggregates + cement + marble sludge | +2/3 of water | + 1/3 of water mixed with the superplasticizer | SCC on the fresh state | SCC2 procedure 2 | Aggregates + cement | + Grout MSG2 (100 kg of sludge dispersed in 80 L of water) | + 120 L of water mixed with the superplasticizer | SCC3 procedure 3 | Aggregates + cement | + Grout MSG4 (100 kg of sludge dispersed in 120 L of water) | + 80 L of water mixed with the superplasticizer | SCC4 procedure 4 | Aggregates + Cement | + Grout MSG8 (100 kg of sludge dispersed in 200 L of water + superplasticizer) | 2/3 | 1/3 |
|
|