Research Article
Mechanical and Durability Properties of Induction-Furnace-Slag-Incorporated Recycled Aggregate Concrete
Table 3
Concrete mix design (quantity for 1 m3of concrete).
| Target strength (MPa) | Coarse aggregate ratio | Cement | Sand | RA | IFS | Water | RA (%) | IFS (%) | (kg) | (kg) | (kg) | (kg) | (kg) |
| 17.23 | 100 | 0 | 237.35 | 893.87 | 955.73 | 0 | 178.22 | 75 | 25 | 237.35 | 968.43 | 682.78 | 227.59 | 178.22 | 50 | 50 | 237.35 | 984.18 | 456.37 | 456.37 | 178.22 | 25 | 75 | 237.35 | 993.52 | 227.62 | 682.85 | 178.22 | 0 | 100 | 237.35 | 990.53 | 0 | 966.16 | 178.22 |
| 20.68 | 100 | 0 | 259.51 | 875.57 | 955.73 | 0 | 178.22 | 75 | 25 | 259.51 | 950.13 | 682.78 | 227.59 | 178.22 | 50 | 50 | 259.51 | 965.88 | 456.37 | 456.37 | 178.22 | 25 | 75 | 259.51 | 975.23 | 227.62 | 682.85 | 178.22 | 0 | 100 | 259.51 | 972.23 | 0 | 966.16 | 178.22 |
| 24.13 | 100 | 0 | 283.75 | 855.57 | 955.73 | 0 | 178.22 | 75 | 25 | 283.75 | 930.13 | 682.78 | 227.59 | 178.22 | 50 | 50 | 283.75 | 945.88 | 456.37 | 456.37 | 178.22 | 25 | 75 | 283.75 | 955.22 | 227.62 | 682.85 | 178.22 | 0 | 100 | 283.75 | 952.23 | 0 | 966.16 | 178.22 |
|
|