Research Article
Compressive Strength and Microstructure Properties of Alkali-Activated Systems with Blast Furnace Slag, Desulfurization Slag, and Gypsum
| | CaO (%) | SiO2 (%) | Al2O3 (%) | Fe2O3 (%) | MgO (%) | Na2O (%) | K2O (%) | SO3 (%) | C (%) | Density (g/cm3) |
| OPC (O) | 62.2 | 20.7 | 6.2 | 3.10 | 2.8 | 0.10 | 0.8 | 2.1 | — | 3.15 | BFS (B) | 43.5 | 32.8 | 15.6 | 0.50 | 4.41 | 0.25 | 0.49 | 1.04 | — | 2.98 | DS (D) | 62.2 | 10.6 | 1.21 | 11.6 | 1.5 | 0.10 | — | 5.2 | 4.1 | 3.01 | Gypsum (G) | 41.6 | 0.73 | 0.17 | 0.16 | — | 0.02 | 0.03 | 55.5 | — | 2.93 |
|
|