| Mixtures | Materials proportions1 | Cement (kg) | Waste | Sand (kg) | Water (kg) | SP (kg) | VMA (kg) | Porcelain (kg) | Ceramic (kg) |
| Reference | 1.00 : 0.00 : 2 : 0.7 | 3.00 | — | — | 6.00 | 2.10 | 0.015 | 0.027 | P15 | 0.85 : 0.15 : 2 : 0.7 | 2.55 | 0.45 | — | 6.00 | 2.10 | 0.015 | 0.027 | P25 | 0.75 : 0.25 : 2 : 0.7 | 2.25 | 0.75 | — | 6.00 | 2.10 | 0.015 | 0.027 | P50 | 0.50 : 0.50 : 2 : 0.7 | 1.50 | 1.50 | — | 6.00 | 2.10 | 0.015 | 0.027 | C15 | 0.85 : 0.15 : 2 : 0.7 | 2.55 | — | 0.45 | 6.00 | 2.10 | 0.015 | 0.027 | C25 | 0.75 : 0.25 : 2 : 0.7 | 2.25 | — | 0.75 | 6.00 | 2.10 | 0.015 | 0.027 | C50 | 0.50 : 0.50 : 2 : 0.7 | 1.50 | — | 1.50 | 6.00 | 2.10 | 0.015 | 0.027 |
|
|