Research Article
Crack Risk Evaluation of Submerged Concrete Tunnel during Hardening Phase
Table 8
Tensile strength at 14 days after casting.
| Concrete | ft28 (N/mm2) | Maturity time at 14 days after casting (days) | Tensile strength at critical time (N/mm2) |
| SV40 | 3.86 | 22.2 | 3.79 | 40% FA | 3.32 | 20.7 | 3.19 | 60% FA | 3.00 | 22.5 | 2.91 | 60% FA-11°C | 3.00 | 19.7 | 2.86 | 40% BFS | 3.89 | 20.7 | 3.74 | 60% BFS | 3.34 | 21.0 | 3.20 |
|
|