Mix proportions of SCC mixtures.
| Mixtures | Cement (kg/m3) | LP (kg/m3) | MP (kg/m3) | w/p | w/c | Water (lt/m3) | CSI (kg/m3) | CSII (kg/m3) | Sand (kg/m3) | Pigment (kg/m3) |
| M1 | 420 | 180 | — | 0.29 | 0.42 | 176 | 507 | 321 | 789 | — | M2 | 420 | — | 180 | 0.29 | 0.42 | 176 | 497 | 315 | 795 | — | M3 | 420 | 180 | — | 0.29 | 0.42 | 176 | 491 | 311 | 807 | 4.20 | M4 | 420 | 180 | — | 0.29 | 0.42 | 176 | 485 | 307 | 816 | 8.40 | M5 | 420 | 180 | — | 0.29 | 0.42 | 176 | 505 | 320 | 791 | 12.60 | M6 | 420 | 180 | — | 0.29 | 0.42 | 176 | 503 | 319 | 792 | 16.80 | M7 | 420 | 180 | — | 0.29 | 0.42 | 176 | 501 | 318 | 799 | 21.00 | M8 | 420 | 180 | — | 0.29 | 0.42 | 176 | 505 | 320 | 793 | 25.20 | M9 | 420 | 180 | — | 0.29 | 0.42 | 176 | 503 | 319 | 788 | 29.40 | M10 | 420 | 180 | — | 0.29 | 0.42 | 176 | 502 | 317 | 791 | 33.60 |
|
|