The Use of Waste Maroon Marble Powder and Iron Oxide Pigment in the Production of Coloured Self-Compacting Concrete
Table 4
Water absorption values of SCC series.
| Water absorption (%) | Mixture | 3 days | 7 days | 28 days |
| M1 | 3.2509 | 2.879 | 2.801 | M2 | 3.2527 | 2.881 | 2.799 | M3 | 3.2520 | 3.059 | 3.028 | M4 | 3.2935 | 2.999 | 2.980 | M5 | 3.3100 | 3.066 | 3.091 | M6 | 3.3538 | 3.145 | 3.108 | M7 | 3.4841 | 3.177 | 3.100 | M8 | 3.6199 | 3.218 | 3.168 | M9 | 3.7106 | 3.310 | 3.225 | M10 | 3.8925 | 3.480 | 3.364 |
|
|