Research Article
The Use of Waste Maroon Marble Powder and Iron Oxide Pigment in the Production of Coloured Self-Compacting Concrete
Table 6
Abrasion depths and mass losses of SCC series.
| Mixtures | M1 | M2 | M3 | M4 | M5 | M6 | M7 | M8 | M9 | M10 |
| 7 days (curing time) | | | | | | | | | | | Depth of abrasion (mm) | 0.90 | 1.1 | 1.3 | 1.2 | 1.5 | 1.5 | 2.0 | 2.1 | 2.2 | 2.0 | Mass loss (%) | 0.95 | 0.97 | 0.98 | 0.96 | 1.13 | 1.25 | 1.26 | 1.46 | 1.73 | 2.34 | 28 days (curing time) | | | | | | | | | | | Depth of abrasion (mm) | 0.90 | 1.3 | 0.90 | 1.1 | 1.2 | 1.0 | 1.5 | 2.1 | 2.0 | 1.8 | Mass loss (%) | 0.90 | 0.92 | 0.91 | 0.89 | 1.11 | 1.18 | 1.21 | 1.38 | 1.59 | 2.12 |
|
|