Research Article
Bond Strength between Glass Fiber Fabrics and Low Water-to-Binder Ratio Mortar: Experimental Characterization
Table 4
Mix proportions during primary tests.
| Test mix | Cement | Silica fume | Sand | Quartz fillers | SP (solid + water) | W/C | W/B | Amount | Type | Amount | (100 µm–600 µm) | EHK | Amount |
| PR1 | 1 | SR | 0.25 | 0.6 | 0.2 | 0.06 | 0.26 | 0.20 | PR2 | 1 | SR | 0.25 | 0.6 | 0.2 | 0.06 | 0.28 | 0.22 | PR3 | 1 | SR | 0.25 | 0.6 | 0.2 | 0.06 | 0.31 | 0.24 | PR4 | 1 | SR | 0.25 | 0.6 | 0.2 | 0.06 | 0.33 | 0.26 |
|
|