Research Article
An Experimental Investigation of the Progressive Failure of Sandstone and Its Energy Evolution Characteristics
Table 2
Crack parameters of the sandstone specimens.
| Sample | (10−3) | (MPa) | (MPa) | (10−3) | (10−3) | | | |
| S60-1 | 2.344 | 28.32 | 72.84 | 2.704 | 0.359 | 0.867 | 0.357 | 0.919 | S60-2 | 1.645 | 33.63 | 76.75 | 2.229 | 0.584 | 0.738 | 0.394 | 0.898 | S100-1 | 1.594 | 34.19 | 80.57 | 1.792 | 0.198 | 0.890 | 0.382 | 0.900 | S100-2 | 1.853 | 36.20 | 69.46 | 2.106 | 0.253 | 0.880 | 0.451 | 0.865 | S100-3 | 1.323 | 43.14 | 107.5 | 1.949 | 0.626 | 0.679 | 0.318 | 0.793 | S100-4 | 1.134 | 60.84 | 130.7 | 1.572 | 0.438 | 0.721 | 0.360 | 0.772 | S100-5 | 0.893 | 61.76 | 150.8 | 1.608 | 0.715 | 0.555 | 0.306 | 0.747 | S120-1 | 2.053 | 38.96 | 68.56 | 2.163 | 0.110 | 0.949 | 0.522 | 0.919 | S120-2 | 1.847 | 39.49 | 69.41 | 1.989 | 0.142 | 0.929 | 0.550 | 0.967 |
|
|