Research Article
Consolidated Undrained Triaxial Compression Tests and Strength Criterion of Solidified Dredged Materials
Table 4
Values of parameters for strength criterion verification.
| Mixing proportion | Curing period | m | n | qu (kPa) | σvy (kPa) | (°) |
| 2.5W+C100+P40 | 28 | 3 | 0.3 | 392 | 510 | 18 | 3.0W+C100+P70 | 28 | 3 | 0.3 | 305 | 436 | 16 | 3.0W+C200 | 28 | 3 | 0.3 | 426 | 559 | 18 | 3.0W+C200+P50 | 28 | 3 | 0.1 | 621 | 760 | 18 |
|
|