Research Article
Cracking and Failure in Rock Specimen Containing Combined Flaw and Hole under Uniaxial Compression
Table 1
Arrangement of specimens.
| Series | Specimen type | α (°) | Sample ID |
| I | Intact specimen (Figure 1(a)) | — | — | II | Single-hole specimen without flaw (Figure 1(b)) | — | SHWF | III | Single-hole and two-flaw specimen (Figure 1(c)) | 0 | SHTF-0 | 30 | SHTF-30 | 60 | SHTF-60 | 90 | SHTF-90 | IV | Two-hole specimen without flaw (Figure 1(d)) | — | THWF | V | Two-hole and single-flaw specimen (Figure 1(e)) | 0 | THSF-0 | 30 | THSF-30 | 60 | THSF-60 | 90 | THSF-90 |
|
|