Research Article
Tension Test for Axially Vibrated Prestressing Fine-Rolled Screw-Threaded Steel Bars Based on Thread-Contact Connection
Table 4
The parameters used in and the frequencies measured from the field test.
| Number | (m) | (m) | Effective tension (kN) | Measured frequency (Hz) |
| 1 | 0.120 | 2.517 | 98.3 | 498 | 2 | 0.123 | 2.517 | 196.5 | 556 | 3 | 0.127 | 2.517 | 317.6 | 616 | 4 | 0.121 | 2.517 | 78.3 | 478 | 5 | 0.124 | 2.527 | 220.3 | 568 | 6 | 0.128 | 2.527 | 307.6 | 603 | 7 | 0.106 | 2.527 | 110.2 | 514 | 8 | 0.109 | 2.527 | 196.5 | 550 | 9 | 0.112 | 2.537 | 327.6 | 629 | 10 | 0.104 | 2.537 | 98.3 | 493 | 11 | 0.108 | 2.537 | 210.8 | 585 | 12 | 0.113 | 2.537 | 327.6 | 622 | 13 | 0.087 | 2.547 | 65.6 | 488 | 14 | 0.161 | 2.547 | 196.5 | 547 | 15 | 0.104 | 2.547 | 262.1 | 585 | 16 | 0.113 | 2.547 | 317.6 | 605 |
|
|