Research Article
Nondestructive Evaluation of FRP-Concrete Interface Bond due to Surface Defects
Table 6
Total delaminated areas due to voids.
| Sample | Actual voided area induced (mm2) | Estimated debonded area (mm2) | Percent difference | Percentage debonding of the total CFRP area |
| 1 | N/A | 0 | N/A | 0 | 2 | N/A | 92 | N/A | 0.05 | 3 | 400 | 550 | 25 | 0.3 | 4 | 1600 | 2064 | 20 | 1.1 | 5 | 800 | 1161 | 29 | 0.6 | 6 | 3200 | 4194 | 21 | 2.3 | 7 | N/A | 460 | N/A | 0.25 | 8 | N/A | 515 | N/A | 0.27 | 9 | N/A | 3675 | N/A | 2.0 | 10 | N/A | 3866 | N/A | 2.1 | 11 | N/A | 1947 | N/A | 1.0 |
|
|