Damage of the bed plate under temperature load after different service times.
| | Damage under condition 1 | Damage under condition 2 | Total damage |
| 1 year | 5.16 × 10−5 | 5.78 × 10−6 | 5.83 × 10−5 | 3 years | 1.55 × 10−4 | 1.73 × 10−5 | 1.72 × 10−4 | 5 years | 2.58 × 10−4 | 2.89 × 10−5 | 2.87 × 10−4 | 10 years | 5.16 × 10−4 | 5.78 × 10−5 | 5.74 × 10−4 | 20 years | 1.03 × 10−3 | 1.15 × 10−4 | 1.15 × 10−3 | 30 years | 1.55 × 10−3 | 1.73 × 10−4 | 1.72 × 10−3 | 40 years | 2.06 × 10−3 | 2.31 × 10−4 | 2.29 × 10−3 | 50 years | 2.58 × 10−3 | 2.89 × 10−4 | 2.87 × 10−3 | 60 years | 3.10 × 10−3 | 3.47 × 10−4 | 3.45 × 10−3 |
|
|