Research Article

Damage Evolution Characteristics of Rock Salt under Different Stress Conditions

Figure 10

Failure patterns of rock salt under different confining pressures. (a) σ3 = 0 MPa. (b) σ3 = 5 MPa. (c) σ3 = 10 MPa. (d) σ3 = 15 MPa. (e) σ3 = 20 MPa. (f) σ3 = 30 MPa. (g) σ3 = 40 MPa.
(a)
(b)
(c)
(d)
(e)
(f)
(g)