Research Article
Characterization of Short-Term Strength Properties of Fiber/Cement-Modified Slurry
Table 2
Calculated results of parameters in BP neural network.
| Cement (c) and fiber (f) contents | a1 | a2 | a3 | a4 | a5 | a6 | a7 | Average error (kPa) |
| 5%c | 27.3 | −1.28 | 9.72 | −2228896 | −0.94 | −10.98 | 12.38 | 0.16 | 10%c | 173 | −1.05 | 3.07 | 2516991 | 1.11 | 9.6 | −2516987 | 1.37 | 15%c | −135.6 | 2.12 | −6.68 | −332.9 | −3.53 | 0.32 | 194.6 | 0.61 | 20%c | −188.8 | 0.77 | −2.19 | 421 | 2.38 | −0.45 | −138.9 | 2.71 | 25%c | 366.7 | −1.58 | 7.55 | −14359490 | −1.11 | −10.32 | 95.3 | 0.32 | 30%c | 344.4 | −1.17 | 5.9 | 578 | 2 | −1.61 | −443.6 | 0.19 | 20%c + 0.25%f | 258.3 | −1.09 | 5 | −5265 | −0.79 | −2.77 | 38.87 | 0.17 | 20%c + 0.5%f | 269.4 | −1.18 | 4.66 | 727.6 | 1.53 | 0.11 | −659 | 0.37 | 20%c + 0.75%f | 195.4 | −1.08 | 5.66 | 581.3 | 1.26 | 0.035 | −511 | 2.04 | 20%c + 1%f | 7227669 | 1.55 | 9.85 | 310 | −1.17 | 3.36 | −7227592 | 0.64 |
|
|