Research Article
Properties of Degraded Waste PET-Modified Styrene-Acrylic Emulsions for Cement Slurry Materials
Figure 17
SEM of the solidified cement slurry test blocks. Polymer content: (a) 0%, (b) 2.5%, (c) 5%, (d) 7.5%, and (e) 10%.
(a) |
(b) |
(c) |
(d) |
(e) |