Experimental Study on Dynamic Performance of Self-Compacting Lightweight Aggregate Concrete under Compression
Table 1
The ingredient radio of concrete.
The mass of each ingredient in 1 cubic meter of concrete (kg)
Concrete strength
Cement
Water
Coarse aggregate/shale ceramsite
Fine aggregate
Mineral powder
Water-reducing agent
C30
461
175
1252
512
—
—
LC30
460
200
670
650
—
—
SCLC30
388
197
300
710
166
8.32
We are committed to sharing findings related to COVID-19 as quickly as possible. We will be providing unlimited waivers of publication charges for accepted research articles as well as case reports and case series related to COVID-19. Review articles are excluded from this waiver policy. Sign up here as a reviewer to help fast-track new submissions.