Research Article
Long-Term Deformation Analysis of Recycled Construction Waste Subgrade Filler
Table 10
Cc and Cu indicators of construction waste samples.
| Condition | Cc | Cu |
| After creep test | 38.59 | 17.5 | 2.6 | 55.14 | 17.8 | 2.7 | 71.68 | 18.1 | 2.7 | 88.22 | 18.2 | 2.8 | 104.76 | 18.4 | 2.9 | After compaction | Upper layer | 14.2 | 2.5 | Middle layer | 17.1 | 2.6 | Lower layer | 18.7 | 2.9 |
|
|