Research Article
Experimental Study on Corrosion of Anchored Rock Mass for Half-Through Intermittent Joints
| Loading time | Theoretical corrosion | 30° angle specimen | 45° angle specimen | Initial mass (g) | Quality after corrosion (g) | Mass loss (g) | Initial mass (g) | Quality after corrosion (g) | Mass loss (g) |
| 24 | 0.0251 | 42.947 | 42.906 | 0.041 | 43.666 | 43.620 | 0.046 | 36 | 0.0376 | 43.237 | 43.181 | 0.056 | 42.946 | 42.892 | 0.054 | 48 | 0.0501 | 43.577 | 43.497 | 0.08 | 43.128 | 43.045 | 0.083 | 60 | 0.0626 | 43.483 | 43.387 | 0.096 | 43.331 | 43.237 | 0.094 | 72 | 0.0752 | 42.913 | 42.804 | 0.109 | 43.508 | 43.405 | 0.103 | 84 | 0.0877 | 43.437 | 43.320 | 0.117 | 42.255 | 42.130 | 0.125 | 96 | 0.1002 | 43.317 | 43.175 | 0.142 | 42.528 | 42.392 | 0.136 | 108 | 0.1128 | 43.283 | 43.283 | 0.171 | 44.404 | 44.243 | 0.161 |
|
|