Research Article
Full-Scale Testing of Precast Concrete Bridge Using Internal Connector in Negative Moment Region
Table 2
Tensile properties of concrete materials.
| Tension stiffening | Tension damage | Stress (MPa) | Inelastic strain | Damage T | Inelastic strain |
| 1.199358 | 0 | 0 | 0 | 1.7052 | 1.99e − 5 | 0 | 1.99e − 5 | 1.121886 | 9.62e − 5 | 0.24384 | 9.62e − 5 | 0.5176338 | 0.00017 | 0.41783 | 0.00017 | 0.1357524 | 0.00041 | 0.55223 | 0.00041 | 0.0339456 | 0.00065 | 0.58806 | 0.00065 |
|
|