Chord rotations of SRC coupling beams at different performance levels (rad).
| Specimen number | Performance level | Being basically intact | Slight damage | Moderate damage | Severe damage |
| Beam1 | 0.0055 | 0.0157 | 0.0264 | 0.0562 | Beam2 | 0.0053 | 0.0137 | 0.0212 | 0.0426 | Beam3 | 0.0060 | 0.0143 | 0.0235 | 0.0446 | Beam4 | 0.0051 | 0.0145 | 0.0239 | 0.0504 | Beam5 | 0.0054 | 0.0149 | 0.0257 | 0.0526 | Beam6 | 0.0051 | 0.0133 | 0.0228 | 0.0403 | Beam7 | 0.0050 | 0.0130 | 0.0228 | 0.0390 |
|
|